Rubber compound 7-IRP-1348 - raw rubber based on a combination of isoprene and divinyl synthetic rubbers.
Purpose of Rubber Compound 7-IRP-1348
Rubber compound 7-IRP-1348 is used for the production of rubber-metal and rubber shock absorbers operating in an air environment within a temperature range from -55°C to +80°C.
Minimum Batch of Rubber Compound 7-IRP-1348
Orders for rubber compound 7-IRP-1348 are accepted in volumes starting from 65 kg.
Rubber Characteristics | Unit | Value |
Tensile Strength | MPa | not less than 12.3 |
Elongation at Break | % | not less than 300 |
Hardness Shore A | Shore A units | 65 - 75 |
Residual Compression Set in Air at 30%, 70°C, 24 hours | % | not more than 40 |
Change in Elongation After Aging in Air at 100°C, 72 hours | % | -75 ... 20 |
Coefficient of Frost Resistance by Recovery After 20% Compression at -55°C | not less than 0.2 | - |
Bond Strength Between Rubber and Metal During Tear | MPa | not less than 3.9 |
Operating Temperature Range | °C | -55 ... +80 |
The price of rubber compound 7-IRP-1348 - upon request.
Color of the rubber compound - black.