Rubber compound 7-IRP-1347 - raw rubber based on a combination of isoprene and divinyl synthetic rubbers.
Rubber compound 7-IRP-1347 is used for the production of rubber-metal and rubber shock absorbers operating in an air environment within a temperature range from -50°C to +70°C.
Orders for rubber compound 7-IRP-1347 are accepted in volumes starting from 65 kg.
Rubber Characteristics | Unit | Value |
Tensile Strength | MPa | not less than 16.7 |
Elongation at Break | % | not less than 550 |
Hardness Shore A | Shore A units | 45 - 60 |
Residual Compression Set in Air at 20%, 100°C, 24 hours | % | not more than 45 |
Brittleness Temperature | °C | not higher than -55 |
Operating Temperature Range | °C | -50 to +70 |
The price of rubber compound 7-IRP-1347 - upon request.
Color of the rubber compound - black.