PURPOSE OF RUBBER COMPOUND 295-T3
Heat-resistant rubber compound 295-T3 is used for the production of molded and non-molded rubber technical items (RTI) that operate in environments such as gasoline, petroleum fuel, industrial and transmission oils, and alcohols within a temperature range from -20°C to +250°C.
Rubber Characteristics | Unit | Value |
Tensile Strength | MPa | not less than 11.0 |
Elongation at Break | % | not less than 400 |
Hardness Shore A | Shore A units | 60 - 75 |
Tensile Strength After Aging in Air at 125°C for 168 hours, not less than | MPa | 10 |
Elongation After Aging in Air at 125°C for 168 hours, not less than | 300 | - |
Volume Loss Due to Abrasion, mm³, not more than | 200 | - |
Operating Temperature Range | °C | -20 to +250 |
The price of rubber compound 295-T3 - upon request