PURPOSE OF RUBBER COMPOUND 2-616: for rubberizing and gumming of rollers, oil and fuel resistant.
Rubber Characteristics | Unit | Value |
Conditional tensile strength, not less than | MPa | 9.8 |
Elongation at break | % | 200 |
Hardness Shore A | Shore A units | 70-85 |
Operating temperature range | °C | Up to +100 |
The price of rubber compound 2-616 - upon request.
Color of the rubber compound - red.